United Cast Bar is the home of Unibar Continuous Cast Iron, produced in two of Europe's most prestigious foundries and distributed through the United Cast Bar distribution network.Unibar continuous cast iron is available in a range of grades, both in flake and spheroidal graphite to suit the application's demands. Produced in rounds, squares and rectangles as standard, and shapes specifically cast to the customer's requirements.
Sede
Chesterfield, Derbyshire, United Kingdom
Sitio web
Tipo
Manufacturer, Processor and Distributor
Certifications
ISO 9001
, ISO 14001
, IATF 16949
, ISO 50001
Grade | Shape | ||
---|---|---|---|
Unibar 200 | Profile, Bar | EN GJL-200C, EN GJL-200 | DIN EN 16482, BS EN 1561 |
Unibar 250 | Profile, Bar | EN GJL-250C, EN GJL-250 | DIN EN 16482, BS EN 1561 |
Unibar 250+ | Profile, Bar | EN GJL-250C, EN GJL-250 | DIN EN 16482, BS EN 1561 |
Unibar 300 | Profile, Bar | EN GJL-300C, EN GJL-300 | DIN EN 16482, BS EN 1561 |
Unibar 350 | Profile, Bar | EN GJL-350 | BS EN 1561 |
Unibar 400-15 | Profile, Bar | EN GJS-400-15C, EN GJS-400-15 | DIN EN 16482, BS EN 1563 |
Unibar 400-18 | Profile, Bar | EN GJS-400-18C, EN GJS-400-18 | DIN EN 16482, BS EN 1563 |
Unibar 400-18LT | Profile, Bar | EN GJS-400-18-LT | DIN EN 16482, BS EN 1563 |
Unibar 500+ | Profile, Bar | EN GJS-500-7C, EN GJS-500-7 | DIN EN 16482, BS EN 1563 |
Unibar 500-7 | Profile, Bar | EN GJS-500-7C, EN GJS-500-7 | DIN EN 16482, BS EN 1563 |