Vimetco is a globally integrated aluminium Group, with bauxite mines in Sierra Leone, coal mines, aluminium production and processing facilities and electricity plant in China and with alumina refinery and aluminium smelter in Romania. The Company’s strategy is focused on expanding added value areas of the business as well as securing its raw material and energy needs.
Sede
Bucharest, Romania
Sitio web
Tipo
Fabricante y procesador
Grade | Shape | ||
---|---|---|---|
EN AW-1050A | Slab | EN AW-1050A | EN 573-3, ASTM E1251 |
EN AW-1070A | Slab | EN AW-1070A | EN 573-3, ASTM E1251 |
EN AW-1350 | Slab | EN AW-1350 | EN 573-3, ASTM E1251 |
EN AW-1370 | Wire, Rod | EN AW-1370, DIN Al99.7 | EN 573-3 |
EN AW-2014 | Slab | EN AW-2014 | EN 573-3, ASTM E1251 |
EN AW-2017A | Slab | EN AW-2017A | EN 573-3, ASTM E1251 |
EN AW-2024 | Slab | EN AW-2024 | EN 573-3, ASTM E1251 |
EN AW-3003 | Slab | EN AW-3003 | EN 573-3, ASTM E1251 |
EN AW-3004 | Slab | EN AW-3004 | EN 573-3, ASTM E1251 |
EN AW-3103A | Slab | EN AW-3103A | EN 573-3, ASTM E1251 |