Production Metal is a family-owned business started in 1969 by Harry Bout. His son Richard Bout began Golden Triangle Specialty Metals in 1982. His youngest son Henry Bout took over Production Metal in 1997. Both businesses are now run by Henry and his dedicated staff following Richard’s untimely death in 2006 due to a snowmobile accident. Harry, the founder of this successful family business, passed away in 2009.
Sede
Cambridge,Ont, Canada
Sitio web
Tipo
Processor and Distributor
Grade | Shape | ||
---|---|---|---|
AISI 1141 | Bar, Plate, Profile | AISI 1141 | |
ASTM 1018 | Bar | ASTM 1018 | |
ASTM 1045 | Bar, Plate, Profile | ASTM 1045 | |
ASTM 1117 | Bar, Plate, Profile | ASTM 1117 | |
ASTM 12L14 | Bar | ASTM 12L14 | |
ASTM 304 | Plate, Bar | ASTM 304, ASTM 304L | |
ASTM 316 | Plate, Bar | ASTM 316, ASTM 316L | |
ASTM 4140 | Bar | ASTM 4140 | |
CSA 44W | Bar, Plate, Profile | CSA 44W | |
CSA 50W | Bar, Plate, Profile | CSA 50W | |