Grade | Shape | ||
---|---|---|---|
EN 1.0302 | Bar | EN 1.0302, DIN C10Pb | |
EN 1.0502 | Bar | EN 1.0502, EN C35Pb | |
EN 1.0503 | Bar | EN 1.0503, EN C45 | |
EN 1.0504 | Bar | EN 1.0504, EN C45Pb | |
EN 1.0540 | Bar | EN 1.0540, EN C50 | |
EN 1.0715 | Bar | EN 1.0715, EN 1.0736, EN 11SMn30, EN 11SMn37 | |
EN 1.0718 | Bar | EN 1.0718, EN 1.0737, EN 11SMnPb30, EN 11SMnPb37 | |
EN 1.0726 | Bar | EN 1.0726, EN 1.0756, EN 35S20, EN 35SPb20 | |
EN 1.0727 | Bar | EN 1.0727, EN 1.0757, EN 45S20, EN 45SPb20 | |
EN 1.0739 | Bar | EN 1.0739, EN 11SMnPb37 | |