Description

EZCast™ Alloys: Highly customizable in achieving a wide range of mechanical properties by optimizing chemistry and heat treatment practices for specific applications. C60K: Improvement on AA365 with lower Si, Fe and Mn levels adjusted to improve elongation, die life, and die sticking.

Ashby charts

Properties

General

Density ρ

2.64 g/cm³ at 20 °C

Mechanical

Elastic modulus E

70 - 74 GPa at 20 °C

Elongation A

18 - 23 % at 20 °C

Tensile strength Rm

205 - 235 MPa at 20 °C

Yield strength YS

100 - 120 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2.1E-5 1/K at 20 °C

measured from 20-300°C

Melting point Tm

552 - 608 °C

Thermal conductivity λ

135 - 170 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Al

-

balance

Si

6 - 9 %

Mg

0.15 - 0.8 %

Mn

0.1 - 0.8 %

Fe

0 - 0.2 %

More

Technological properties

Application areas

Crash-resistant structural components for automotive applications, engine cradles, cross-members, side doors, radiator mounting, engine mounts, sub-frames, brackets, shock towers and tunnels

Corrosion properties

excellent corrosion resistance

Processing history

Temper: T4

Processing methods

Good castability, reduced die sticking, suitable for high pressure die cast (HPDC) and vacuum die casting (VDC)

This material data has been provided by Alcoa.