EN 573-3 Grade AW-5050 H49

Want to keep this datasheet? Save it now in your required format

Description

Material EN AW-Al Mg1,5(C) is produced for sheet metal, strip and plates. It is food-safe and it is used for prematerial for cans, caps and stoppers.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.68 - 2.69 g/cm³

Show Material materials with Density of 2.68 - 2.69 g/cm³

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

69 - 70 GPa

Show Material materials with Elastic modulus of 69 - 70 GPa

Elongation A50

20.0 °C

1 - 2 %

Show Material materials with Elongation A50 of 1 - 2 %

23.0 °C

1 - 2 %

Show Material materials with Elongation A50 of 1 - 2 %

Elongation A50, transverse

20.0 °C

1 - 2 %

Show Material materials with Elongation A50, transverse of 1 - 2 %

Plane-Strain Fracture Toughnes

23.0 °C

22 - 35 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

23.0 °C

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 5000 Series Aluminium

Shear modulus

23.0 °C

26 - 26.5 GPa

Show Material materials with Shear modulus of 26 - 26.5 GPa

Typical for Wrought 5000 Series Aluminium

Tensile strength

20.0 °C

240 MPa

Show Material materials with Tensile strength of 240 MPa

23.0 °C

240 MPa

Show Material materials with Tensile strength of 240 MPa

Unlock all property charts

Tensile strength, transverse

20.0 °C

240 MPa

Show Material materials with Tensile strength, transverse of 240 MPa

Yield strength Rp0.2

20.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2 of 220 MPa

23.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2 of 220 MPa

Unlock all property charts

Yield strength Rp0.2, transverse

20.0 °C

220 MPa

Show Material materials with Yield strength Rp0.2, transverse of 220 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

20.0 °C

2.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K

100.0 °C

2.38E-5 1/K

Show Material materials with Coefficient of thermal expansion of 2.38E-5 1/K

Unlock all property charts

Max service temperature

150 °C

Show Material materials with Max service temperature of 150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

620 - 650 °C

Show Material materials with Melting point of 620 - 650 °C

Specific heat capacity

23.0 °C

879 - 963 J/(kg·K)

Show Material materials with Specific heat capacity of 879 - 963 J/(kg·K)

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

23.0 °C

170 - 193 W/(m·K)

Show Material materials with Thermal conductivity of 170 - 193 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical conductivity

23.0 °C

2.30E+7 - 2.90E+7 S/m

Show Material materials with Electrical conductivity of 2.30E+7 - 2.90E+7 S/m

Electrical resistivity

23.0 °C

3.45E-8 - 4.35E-8 Ω·m

Show Material materials with Electrical resistivity of 3.45E-8 - 4.35E-8 Ω·m

Chemical properties

PropertyValue

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

Copper

0.2 %

Show Material materials with Copper of 0.2 %

Iron

0.7 %

Show Material materials with Iron of 0.7 %

Magnesium

1.1 - 1.8 %

Show Material materials with Magnesium of 1.1 - 1.8 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Other

each 0.05, total 0.10, Rest Al

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

Technological properties

Property
Workability

Good workability.