EN 573-1 Grade AW-1350 H19

Want to keep this datasheet? Save it now in your required format

Description

Excellent electrical conductivity.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-1 Grade AW-1350 H19 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.69 - 2.71 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.2 - 3 mm

Mechanical

Plane-Strain Fracture Toughnes

KIC

Typical for Wrought 1000 Series Aluminium

Poisson's ratio

ν

Typical for Wrought 1000 Series Aluminium

Thermal

Coefficient of thermal expansion

α

2.36E-5 - 2.38E-5 1/K at 20 °C

20-100°C

Hide chart

Melting point

Tm

645 - 657 °C

Specific heat capacity

cp

900 - 963 J/(kg·K) at 20 °C

Typical for Wrought 1000 Series Aluminium

Thermal conductivity

λ

138 - 235 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

3.54E+7 - 3.65E+7 S/m at 20 °C

Electrical resistivity

ρel

2.74E-8 - 4.9E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Al

99.5 %

Fe

0.4 %

Other

0.1 %

Ti + V < 0.02, each 0.03, total 0.10

Si

0.1 %

B

0.05 %

More

Technological properties

Anodizing

Good (For surface protection only)

Application areas

Conductors; rods for the manufacture of aluminium conductor wires.

Brazing

Excellent

Corrosion properties

Very Good

Welding

Very Good

Workability

Very Good

This material data has been provided by Aludium,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.