Mechanical

PropertyTemperatureValue

Tensile strength

20.0 °C

160 - 200 MPa

Show Material materials with Tensile strength of 160 - 200 MPa

Chemical properties

PropertyValue

Aluminium

99.5 %

Show Material materials with Aluminium of 99.5 %

Boron

0.05 %

Show Material materials with Boron of 0.05 %

Chromium

0.01 %

Show Material materials with Chromium of 0.01 %

Copper

0.05 %

Show Material materials with Copper of 0.05 %

Gallium

0.03 %

Show Material materials with Gallium of 0.03 %

Iron

0.4 %

Show Material materials with Iron of 0.4 %

Manganese

0.01 %

Show Material materials with Manganese of 0.01 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Zinc

0.05 %

Show Material materials with Zinc of 0.05 %