EN AW-2017A H18 Extruded Tube

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Electrical

Electrical conductivity σel

18 S/m at 20 °C

Electrical resistivity ρel

0.04 Ω·m at 20 °C

General

Density ρ

2.8 g/cm³ at 20 °C

Mechanical

Elastic modulus E

72.5 GPa at 20 °C

Tensile strength Rm

315 MPa at 20 °C

Thermal

Melting point Tm

512 °C

Thermal conductivity λ

130 W/(m·K) at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

3.5 - 4.5 %

Fe

0.7 %

Mn

0.4 - 1 %

Mg

0.4 - 1 %

Zn

0.25 %

More

This material data has been provided by AluKey.