EN AW-2024 T4

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Elongation A

18 % at 20 °C

Elongation A50 A50

12 - 14 % at 20 °C

Hardness, Brinell HB

100 - 120 [-] at 20 °C

Tensile strength Rm

420 - 425 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

260 - 315 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Cu

3.8 - 4.9 %

Mg

1.2 - 1.8 %

Si

0.5 %

Fe

0.5 %

Mn

0.3 - 0.9 %

More

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.