Density ρ
2.81 g/cm³ at 20 °C
Elongation A
8 % at 20 °C
Elongation A50 A50
6 % at 20 °C
Tensile strength Rm
330 - 370 MPa at 20 °C
Yield strength Rp0.2 Rp0.2
210 - 250 MPa at 20 °C
Element
Weight %
Comment
3.3 - 4.5 %
0.8 %
0.8 - 1.5 %
0.7 %
0.5 %