7075-T79511 profile

Want to keep this datasheet? Save it now in your required format

This material data has been provided by Alu Key.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

20.0 °C

2.8 g/cm³

Show Material materials with Density of 2.8 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

20.0 °C

71 GPa

Show Material materials with Elastic modulus of 71 GPa

Thermal

PropertyTemperatureValue

Melting point

480 - 640 °C

Show Material materials with Melting point of 480 - 640 °C

Specific heat capacity

20.0 °C

830 J/(kg·K)

Show Material materials with Specific heat capacity of 830 J/(kg·K)

Thermal conductivity

20.0 °C

135 - 160 W/(m·K)

Show Material materials with Thermal conductivity of 135 - 160 W/(m·K)