Properties

Mechanical

Elongation A

12 % at 20 °C

Elongation A50 A50

20 % at 20 °C

Hardness, Brinell HB

33 [-] at 20 °C

Tensile strength Rm

95 - 160 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

35 - 180 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

1 - 1.5 %

Fe

0.7 %

Si

0.6 %

Zn

0.1 %

Cu

0.05 - 0.2 %