EN 573-3 Grade AW-3003 O3

Want to keep this datasheet? Save it now in your required format

Description

Aluminum EN AW-3003 is a popular alloy that offers customers very good atmospheric corrosion resistance and moderate strength. Aluminum 3003 offers good machinability for aluminum alloys, though it is not heat treatable. Unlike other aluminum alloys, EN AW-3003 is weldable by conventional welding methods. It also takes cold and hot working well and has generally better mechanical properties when compared to 1000 series aluminum alloys.

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.73 g/cm³

Show Material materials with Density of 2.73 g/cm³

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Mechanical

PropertyValueConditionRelated StandardsShapeComment

Elastic modulus

69.0 GPa

Show Material materials with Elastic modulus of 69.0 GPa

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

69.5 GPa

Show Material materials with Elastic modulus of 69.5 GPa

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

26.1 GPa

Show Material materials with Shear modulus of 26.1 GPa

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Tensile strength

95.0 - 120.0 MPa

Show Material materials with Tensile strength of 95.0 - 120.0 MPa

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Thermal

PropertyTemperatureValueConditionRelated StandardsShape

Coefficient of thermal expansion

-50 °C

2.1499999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1499999999999997e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20 °C

2.1499999999999997e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.1499999999999997e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

20 °C

2.52e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.52e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

100 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

200 °C

2.41e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.41e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

300 °C

2.52e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.52e-05 1/K

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Melting point

640.0 - 655.0 °C

Show Material materials with Melting point of 640.0 - 655.0 °C

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

643.0 - 654.0 °C

Show Material materials with Melting point of 643.0 - 654.0 °C

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Specific heat capacity

893.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 J/(kg·K)

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Thermal conductivity

159.0 - 193.0 W/(m·K)

Show Material materials with Thermal conductivity of 159.0 - 193.0 W/(m·K)

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

160.0 - 200.0 W/(m·K)

Show Material materials with Thermal conductivity of 160.0 - 200.0 W/(m·K)

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Electrical

PropertyValueConditionRelated StandardsShape

Electrical conductivity

23000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

24000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 24000000.0 - 29000000.0 S/m

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Electrical resistivity

3.45e-08 - 4.17e-08 Ω·m

Show Material materials with Electrical resistivity of 3.45e-08 - 4.17e-08 Ω·m

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

3.45e-08 - 4.35e-08 Ω·m

Show Material materials with Electrical resistivity of 3.45e-08 - 4.35e-08 Ω·m

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.05 - 0.2 %

Show Material materials with Copper of 0.05 - 0.2 %

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Iron

0.70 %

Show Material materials with Iron of 0.70 %

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Manganese

1.0 - 1.5 %

Show Material materials with Manganese of 1.0 - 1.5 %

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Silicon

0.6 %

Show Material materials with Silicon of 0.6 %

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %

O3

EN 573-3, EN 1715-3

Strip, Sheet, Plate, Foil, Wire, Tube, Bar

Technological properties

Property
Anodizing

decorative: sufficient, Protective: very good

Brazing

hard brazing (with flux/ without flux): very good / very good, friction soldering: very good, soft brazing with flux: very good

Corrosion properties

Seawater: good, weathering: very good

Workability

Bending / Spinning (cold): very good / very good, Impact extrusion (cold): acceptable, Deep drawing / upsetting (Condition) very good (O) / very good (H12)