EN AW-3003 H112

.XLSX
.PDF
Save

Description

Primary standard name

Properties

Mechanical

Elongation A50 A50

10 - 20 % at 20 °C

Hardness, Brinell HB

29 - 35 [-] at 20 °C

Tensile strength Rm

95 - 115 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

35 - 70 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Mn

1 - 1.5 %

Fe

0.7 %

Si

0.6 %

Zn

0.1 %

Cu

0.05 - 0.2 %

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.