Properties

General

Density

ρ

2.72 g/cm³ at 20 °C

Dimension

Dimensions

Durchmesser

Thickness

t

0.2 - 1 mm

Mechanical

Bending angle 180°

θ180

2 °/t at 20 °C

Show 3000 Series materials with Bending angle 180° of 2 °/t at 20 °C

Bending angle 90°

θ90

0.5 - 1.5 °/t at 20 °C

Show 3000 Series materials with Bending angle 90° of 0.5 - 1.5 °/t at 20 °C

Elastic modulus

E

68.6 - 70 GPa at 20 °C

Show 3000 Series materials with Elastic modulus of 68.6 - 70 GPa at 20 °C

Elongation A100

A100

6 % at 20 °C

Show 3000 Series materials with Elongation A100 of 6 % at 20 °C

Elongation A50

A50

1 - 4 % at 20 °C

Show 3000 Series materials with Elongation A50 of 1 - 4 % at 20 °C

Elongation A50, transverse

A50,trans

3 - 4 % at 20 °C

Show 3000 Series materials with Elongation A50, transverse of 3 - 4 % at 20 °C

Hardness, Brinell

HB

66 [-] at 20 °C

Show 3000 Series materials with Hardness, Brinell of 66 [-] at 20 °C

Hardness, HBW

HBW

66 [-] at 20 °C

Show 3000 Series materials with Hardness, HBW of 66 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 3000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 3000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 3000 Series Aluminium

Shear modulus

G

25 - 27 GPa at 20 °C

Show 3000 Series materials with Shear modulus of 25 - 27 GPa at 20 °C

Tensile strength

Rm

190 - 265 MPa at 20 °C

Show 3000 Series materials with Tensile strength of 190 - 265 MPa at 20 °C

Tensile strength, transverse

Rm,trans

220 - 265 MPa at 20 °C

Show 3000 Series materials with Tensile strength, transverse of 220 - 265 MPa at 20 °C

Yield strength

YS

170 MPa at 20 °C

Show 3000 Series materials with Yield strength of 170 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

170 - 180 MPa at 20 °C

Show 3000 Series materials with Yield strength Rp0.2 of 170 - 180 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

170 MPa at 20 °C

Show 3000 Series materials with Yield strength Rp0.2, transverse of 170 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.15E-5 1/K at -50 °C

20-100°C

Hide chart

Melting point

Tm

629 - 655 °C

Specific heat capacity

cp

893 J/(kg·K) at 20 °C

Thermal conductivity

λ

160 - 190 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.00E+7 - 2.50E+7 S/m at 20 °C

Electrical resistivity

ρel

4E-8 - 4.35E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Mn

1 - 1.5 %

Mg

0.8 - 1.3 %

Fe

0.7 %

Si

0.3 %

More

Technological properties

Anodizing

Good (For surface protection only)

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Furniture, Plinths, Blinds: Intermediate transformation/interior use; Heat exchangers: Fins; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Food can: Body, Lids; Semi-rigid and corrugated: Smooth wall

Brazing

Very Good

Corrosion properties

Good

Welding

Very Good

Workability

Good

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.