EN 573-1 Grade AW-3004 H45

Want to keep this datasheet? Save it now in your required format

Description

Stronger than 1200, 3003 and 3103 for similar applications. Good for chemical and food contact applications.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-1 Grade AW-3004 H45 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.72 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.18 - 0.3 mm

Mechanical

Plane-Strain Fracture Toughnes

KIC

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

ν

Typical for Wrought 3000 Series Aluminium

Thermal

Coefficient of thermal expansion

α

2.15E-5 1/K at -50 °C

20-100°C

Hide chart

Melting point

Tm

629 - 655 °C

Specific heat capacity

cp

893 J/(kg·K) at 20 °C

Thermal conductivity

λ

160 - 190 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.00E+7 - 2.50E+7 S/m at 20 °C

Electrical resistivity

ρel

4E-8 - 4.35E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Mn

1 - 1.5 %

Mg

0.8 - 1.3 %

Fe

0.7 %

Si

0.3 %

More

Technological properties

Anodizing

Good (For surface protection only)

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels, Foil for bituminous coating; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Furniture, Plinths, Blinds: Intermediate transformation/interior use; Heat exchangers: Fins; Wind energy: Nacelle coverings, Rotor, Hub, Stairs; Food can: Body, Lids; Semi-rigid and corrugated: Smooth wall

Brazing

Very Good

Corrosion properties

Good

Welding

Very Good

Workability

Good

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.