EN 573-1 Grade AW-3005 O

Want to keep this datasheet? Save it now in your required format

Description

A low to medium strength alloy with moderate corrosion resistance.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-1 Grade AW-3005 O falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.72 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.04 - 2 mm

Mechanical

Bending angle 180°

θ180

0 - 1 °/t at 20 °C

Show 3000 Series materials with Bending angle 180° of 0 - 1 °/t at 20 °C

Bending angle 90°

θ90

0 - 1 °/t at 20 °C

Show 3000 Series materials with Bending angle 90° of 0 - 1 °/t at 20 °C

Elastic modulus

E

69 - 70 GPa at 20 °C

Show 3000 Series materials with Elastic modulus of 69 - 70 GPa at 20 °C

Elongation A100

A100

8 - 10 % at 20 °C

Show 3000 Series materials with Elongation A100 of 8 - 10 % at 20 °C

Elongation A50

A50

1 - 19 % at 20 °C

Show 3000 Series materials with Elongation A50 of 1 - 19 % at 20 °C

Elongation A50, transverse

A50,trans

12 - 19 % at 20 °C

Show 3000 Series materials with Elongation A50, transverse of 12 - 19 % at 20 °C

Hardness, Brinell

HB

33 [-] at 20 °C

Show 3000 Series materials with Hardness, Brinell of 33 [-] at 20 °C

Hardness, HBW

HBW

33 - 73 [-] at 20 °C

Show 3000 Series materials with Hardness, HBW of 33 - 73 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 3000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 3000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 3000 Series Aluminium

Shear modulus

G

26 - 26.5 GPa at 20 °C

Show 3000 Series materials with Shear modulus of 26 - 26.5 GPa at 20 °C

Tensile strength

Rm

115 - 290 MPa at 20 °C

Show 3000 Series materials with Tensile strength of 115 - 290 MPa at 20 °C

Tensile strength, transverse

Rm,trans

115 - 165 MPa at 20 °C

Show 3000 Series materials with Tensile strength, transverse of 115 - 165 MPa at 20 °C

Yield strength

YS

45 MPa at 20 °C

Show 3000 Series materials with Yield strength of 45 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

45 MPa at 20 °C

Show 3000 Series materials with Yield strength Rp0.2 of 45 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

45 MPa at 20 °C

Show 3000 Series materials with Yield strength Rp0.2, transverse of 45 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.32E-5 1/K at 20 °C

20-100°C

Hide chart

Melting point

Tm

630 - 654 °C

Specific heat capacity

cp

893 J/(kg·K) at 20 °C

Thermal conductivity

λ

160 - 200 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

2.30E+7 - 2.80E+7 S/m at 20 °C

Electrical resistivity

ρel

3.8E-8 - 4.35E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Mn

1 - 1.5 %

Fe

0.7 %

Si

0.6 %

Cu

0.3 %

More

Technological properties

Anodizing

Good

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Electronic devices: Housing of devices; Insulation; Cosmetics: Cosmetics pieces

Brazing

Good

Corrosion properties

Good

Welding

Good

Workability

Good

This material data has been provided by Aludium,WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.