EN 573-3 Grade AW-3102 F

Want to keep this datasheet? Save it now in your required format

Description

Naturally hard AlMn alloy. The alloy is not food safe.

Related Standards

Equivalent Materials

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated StandardsShape

Density

2.71 g/cm³

Show Material materials with Density of 2.71 g/cm³

F

EN 573-3, EN 570, EN 755

Strip, Sheet, Plate, Tube, Bar

Mechanical

PropertyTemperatureValueConditionRelated StandardsShapeComment

Elastic modulus

69.5 - 70.0 GPa

Show Material materials with Elastic modulus of 69.5 - 70.0 GPa

Typical for Wrought 3000 Series Aluminium

Elongation

23.0 %

Show Material materials with Elongation of 23.0 %

F

EN 573-3, EN 755

Strip, Sheet, Plate, Tube, Bar

A50

25.0 %

Show Material materials with Elongation of 25.0 %

F

EN 573-3, EN 755

Strip, Sheet, Plate, Tube, Bar

A100

20.0 °C

25.0 %

Show Material materials with Elongation of 25.0 %

F

EN 573-3

Profile, Rod, Tube

Hardness, Brinell

23.0 [-]

Show Material materials with Hardness, Brinell of 23.0 [-]

F

EN 573-3, EN 570, EN 755

Strip, Sheet, Plate, Tube, Bar

20.0 °C

23.0 [-]

Show Material materials with Hardness, Brinell of 23.0 [-]

F

EN 573-3

Profile, Rod, Tube

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 3000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 3000 Series Aluminium

Shear modulus

25.0 - 26.0 GPa

Show Material materials with Shear modulus of 25.0 - 26.0 GPa

Typical for Wrought 3000 Series Aluminium

Tensile strength

80.0 MPa

Show Material materials with Tensile strength of 80.0 MPa

F

EN 573-3, EN 755

Strip, Sheet, Plate, Tube, Bar

20.0 °C

80.0 MPa

Show Material materials with Tensile strength of 80.0 MPa

F

EN 573-3

Profile, Rod, Tube

Thermal

PropertyValueComment

Coefficient of thermal expansion

2.2e-05 - 2.4e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.2e-05 - 2.4e-05 1/K

Typical for Wrought 3000 Series Aluminium

Melting point

629.0 - 654.0 °C

Show Material materials with Melting point of 629.0 - 654.0 °C

Typical for Wrought 3000 Series Aluminium

Specific heat capacity

893.0 - 920.0 J/(kg·K)

Show Material materials with Specific heat capacity of 893.0 - 920.0 J/(kg·K)

Typical for Wrought 3000 Series Aluminium

Thermal conductivity

154.0 - 193.0 W/(m·K)

Show Material materials with Thermal conductivity of 154.0 - 193.0 W/(m·K)

Typical for Wrought 3000 Series Aluminium

Electrical

PropertyValueComment

Electrical conductivity

23000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 23000000.0 - 29000000.0 S/m

Typical for Wrought 3000 Series Aluminium

Electrical resistivity

3.4e-08 - 4.2e-08 Ω·m

Show Material materials with Electrical resistivity of 3.4e-08 - 4.2e-08 Ω·m

Typical for Wrought 3000 Series Aluminium

Chemical properties

PropertyValueConditionRelated StandardsShape

Copper

0.1 %

Show Material materials with Copper of 0.1 %

F

EN 573-3, EN 570, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Iron

0.7 %

Show Material materials with Iron of 0.7 %

F

EN 573-3

Profile, Rod, Tube

0.70 %

Show Material materials with Iron of 0.70 %

F

EN 573-3, EN 570, EN 755

Strip, Sheet, Plate, Tube, Bar

Manganese

0.05 - 0.4 %

Show Material materials with Manganese of 0.05 - 0.4 %

F

EN 573-3, EN 570, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Silicon

0.4 %

Show Material materials with Silicon of 0.4 %

F

EN 573-3, EN 570, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Titanium

0.1 %

Show Material materials with Titanium of 0.1 %

F

EN 573-3, EN 570, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Zinc

0.3 %

Show Material materials with Zinc of 0.3 %

F

EN 573-3, EN 570, EN 755

Profile, Rod, Tube, Strip, Sheet, Plate, Bar

Technological properties

Property
Workability

Good workability.