EN 573-3 Grade AW-4017 H42

Want to keep this datasheet? Save it now in your required format

Description

Age-hardenable AlSi alloy. The alloy is food safe.

Related Standards

Equivalent Materials

Ashby charts

See where EN 573-3 Grade AW-4017 H42 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.72 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Mechanical

Elastic modulus

E

69 - 71 GPa at 20 °C

Show 4000 Series materials with Elastic modulus of 69 - 71 GPa at 20 °C

Typical for Wrought 4000 Series Aluminium

Elongation A50

A50

2 % at 20 °C

Show 4000 Series materials with Elongation A50 of 2 % at 20 °C

Elongation A50, transverse

A50,trans

2 % at 20 °C

Show 4000 Series materials with Elongation A50, transverse of 2 % at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 4000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 4000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 4000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Typical for Wrought 4000 Series Aluminium

Shear modulus

G

26 GPa at 20 °C

Show 4000 Series materials with Shear modulus of 26 GPa at 20 °C

Typical for Wrought 4000 Series Aluminium

Tensile strength

Rm

145 - 200 MPa at 20 °C

Show 4000 Series materials with Tensile strength of 145 - 200 MPa at 20 °C

Tensile strength, transverse

Rm,trans

145 - 200 MPa at 20 °C

Show 4000 Series materials with Tensile strength, transverse of 145 - 200 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

120 MPa at 20 °C

Show 4000 Series materials with Yield strength Rp0.2 of 120 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

120 MPa at 20 °C

Show 4000 Series materials with Yield strength Rp0.2, transverse of 120 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

1.2E-5 - 2.2E-5 1/K at 20 °C

Typical for Wrought 4000 Series Aluminium

Specific heat capacity

cp

864 J/(kg·K) at 20 °C

Typical for Wrought 4000 Series Aluminium

Thermal conductivity

λ

138 - 155 W/(m·K) at 20 °C

Typical for Wrought 4000 Series Aluminium

Electrical

Electrical conductivity

σel

2.30E+7 - 3.00E+7 S/m at 20 °C

Typical for Wrought 4000 Series Aluminium

Electrical resistivity

ρel

3.8E-8 - 5E-8 Ω·m at 20 °C

Typical for Wrought 4000 Series Aluminium

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Fe

0.7 %

Mn

0.6 - 1.2 %

Si

0.6 - 1.6 %

Zn

0.2 %

More

Technological properties

Workability

Moderate Workability

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.