Properties

General

Density

ρ

2.7 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Thickness

t

0.1 - 4 mm

Mechanical

Bending angle 180°

θ180

0 - 1 °/t at 20 °C

Show 5000 Series materials with Bending angle 180° of 0 - 1 °/t at 20 °C

Bending angle 90°

θ90

0 - 1.5 °/t at 20 °C

Show 5000 Series materials with Bending angle 90° of 0 - 1.5 °/t at 20 °C

Elastic modulus

E

69 - 70 GPa at 20 °C

Show 5000 Series materials with Elastic modulus of 69 - 70 GPa at 20 °C

Elongation

A

18 - 20 % at 20 °C

Show 5000 Series materials with Elongation of 18 - 20 % at 20 °C

Elongation A100

A100

8 - 20 % at 20 °C

Show 5000 Series materials with Elongation A100 of 8 - 20 % at 20 °C

Elongation A50

A50

8 - 24 % at 20 °C

Show 5000 Series materials with Elongation A50 of 8 - 24 % at 20 °C

Elongation A50, transverse

A50,trans

15 - 24 % at 20 °C

Show 5000 Series materials with Elongation A50, transverse of 15 - 24 % at 20 °C

Elongation, transverse

A

20 % at 20 °C

Show 5000 Series materials with Elongation, transverse of 20 % at 20 °C

Hardness, Brinell

HB

29 - 30 [-] at 20 °C

Show 5000 Series materials with Hardness, Brinell of 29 - 30 [-] at 20 °C

Hardness, HBW

HBW

29 [-] at 20 °C

Show 5000 Series materials with Hardness, HBW of 29 [-] at 20 °C

Plane-Strain Fracture Toughnes

KIC

22 - 35 MPa·√m at 20 °C

Show 5000 Series materials with Plane-Strain Fracture Toughnes of 22 - 35 MPa·√m at 20 °C

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

0.33 [-] at 20 °C

Show 5000 Series materials with Poisson's ratio of 0.33 [-] at 20 °C

Shear modulus

G

26.1 - 26.5 GPa at 20 °C

Show 5000 Series materials with Shear modulus of 26.1 - 26.5 GPa at 20 °C

Tensile strength

Rm

90 - 150 MPa at 20 °C

Show 5000 Series materials with Tensile strength of 90 - 150 MPa at 20 °C

Tensile strength, transverse

Rm,trans

100 - 145 MPa at 20 °C

Show 5000 Series materials with Tensile strength, transverse of 100 - 145 MPa at 20 °C

Yield strength

YS

35 MPa at 20 °C

Show 5000 Series materials with Yield strength of 35 MPa at 20 °C

Yield strength Rp0.2

Rp0.2

35 - 80 MPa at 20 °C

Show 5000 Series materials with Yield strength Rp0.2 of 35 - 80 MPa at 20 °C

Yield strength Rp0.2, transverse

Rp0.2,trans

35 MPa at 20 °C

Show 5000 Series materials with Yield strength Rp0.2, transverse of 35 MPa at 20 °C

Thermal

Coefficient of thermal expansion

α

2.38E-5 1/K at 20 °C

20-100°C

Hide chart

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

630 - 655 °C

Specific heat capacity

cp

897 J/(kg·K) at 20 °C

Thermal conductivity

λ

200 - 201 W/(m·K) at 20 °C

Electrical

Electrical conductivity

σel

3.00E+7 S/m at 20 °C

Electrical resistivity

ρel

3.3E-8 - 3.33E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Mg

0.5 - 1.1 %

Fe

0.45 - 0.7 %

Si

0.3 %

Zn

0.2 - 0.25 %

More

Technological properties

Anodizing

Excellent (anodizing quality)

Application areas

Facades: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Roofing: Single sheet, Sheets for composites/ sandwich Panels; Doors: Sheets for composites/ sandwich Panels, Sheets for mechanized panels; Sun Protection Systems: Single sheet (covering, sun breakers and gutters); Interiors and ceilings: Single sheet, Sheets for composites/ sandwich Panels, Sheets for mechanized panels, Decoration; Furniture, Plinths, Blinds: Single sheet, Intermediate transformation/interior use; Anodizing quality; Heat exchangers: Fins, General applications; Cosmetics: Cosmetics pieces; Automotive trim: Interior trim; Components: Automotive fins, Heat exchangers

Brazing

Good

Corrosion properties

Excellent

Welding

Very Good

Workability

Very Good

This material data has been provided by Aludium,WIAM,AluKey.