EN 541 Grade AW-5006 H29

Want to keep this datasheet? Save it now in your required format

Description

The material, that not in the standard 573-3: 2003-10 (chemical composition of aluminum and aluminum alloys) are contained, find for rolled products for covers and dose lower parts use.

Related Standards

Equivalent Materials

Ashby charts

See where EN 541 Grade AW-5006 H29 falls on the material property chart for Density against Elastic modulus in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

Density

ρ

2.71 g/cm³ at 20 °C

Dimension

Dimensions

Dicke

Mechanical

Elastic modulus

E

Typical for Wrought 5000 Series Aluminium

Plane-Strain Fracture Toughnes

KIC

Typical for Wrought 5000 Series Aluminium

Poisson's ratio

ν

Typical for Wrought 5000 Series Aluminium

Shear modulus

G

Typical for Wrought 5000 Series Aluminium

Thermal

Coefficient of thermal expansion

α

2.2E-5 - 2.5E-5 1/K at 20 °C

Typical for Wrought 5000 Series Aluminium

Max service temperature

Tmax

150 °C

Typical for Wrought 5000 Series Aluminium

Melting point

Tm

600 - 650 °C

Typical for Wrought 5000 Series Aluminium

Specific heat capacity

cp

879 - 963 J/(kg·K) at 20 °C

Typical for Wrought 5000 Series Aluminium

Thermal conductivity

λ

112 - 205 W/(m·K) at 20 °C

Typical for Wrought 5000 Series Aluminium

Electrical

Electrical conductivity

σel

1.80E+7 - 3.10E+7 S/m at 20 °C

Typical for Wrought 5000 Series Aluminium

Electrical resistivity

ρel

3.3E-8 - 5E-8 Ω·m at 20 °C

Typical for Wrought 5000 Series Aluminium

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15, Rest Al

Fe

0.8 %

Mg

0.8 - 1.3 %

Mn

0.4 - 0.8 %

Si

0.4 %

More

Technological properties

Workability

Good workability.

This material data has been provided by WIAM,AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.