EN 1706 Grade 3.2583 F

.XLSX
.PDF
Save

Description

Related Standards

Equivalent Materials

Properties

General

Density ρ

2.65 g/cm³ at 20 °C

Mechanical

Elastic modulus E

75 GPa at 20 °C

Elongation A50 A50

1 - 2 % at 20 °C

Hardness, Brinell HB

50 - 55 [-] at 20 °C

Poisson's ratio ν

0.33 [-] at 20 °C

Typical for Cast 3xx.x Series Aluminium

Shear modulus G

2.8 GPa at 20 °C

Typical for Cast 3xx.x Series Aluminium

Tensile strength Rm

150 - 170 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

80 - 90 MPa at 20 °C

Thermal

Coefficient of thermal expansion α

2E-5 1/K at 20 °C

Show chart

Melting point Tm

530 - 580 °C

Specific heat capacity cp

890 J/(kg·K) at 20 °C

Thermal conductivity λ

130 - 150 W/(m·K) at 20 °C

Electrical

Electrical conductivity σel

1.60E+7 - 2.20E+7 S/m at 20 °C

Electrical resistivity ρel

4.55E-8 - 6.25E-8 Ω·m at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

each 0.05, total 0.15

Si

10.5 - 13.5 %

Cu

1 %

Fe

0.8 %

Zn

0.5 %

More

Technological properties

Anodizing

decorative: not recommended

Corrosion properties

general: acceptable

General machinability

after thermal treatment: acceptable

This material data has been provided by AluKey.