CEN/TS 13388 Grade 42 3065

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Magnesium

0.05 %

Show Material materials with Magnesium of 0.05 %

Manganese

1.5 - 3 %

Show Material materials with Manganese of 1.5 - 3 %

Nickel

43 - 46 %

Show Material materials with Nickel of 43 - 46 %

Other

Rest Cu, total 0.5

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Zinc

0.1 %

Show Material materials with Zinc of 0.1 %