CEN/TS 13388 Grade C-9232

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Copper

62 - 66 %

Show Material materials with Copper of 62 - 66 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

14 - 16 %

Show Material materials with Nickel of 14 - 16 %

Other

Rest Zn, total 0.3