Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

110 - 130 GPa

Show Material materials with Elastic modulus of 110 - 130 GPa

Typical for Cast Copper High Copper Alloy

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 1/K

Typical for Cast Copper High Copper Alloy

Melting point

835 - 1115 °C

Show Material materials with Melting point of 835 - 1115 °C

Typical for Cast Copper High Copper Alloy

Specific heat capacity

23.0 °C

389 - 420 J/(kg·K)

Show Material materials with Specific heat capacity of 389 - 420 J/(kg·K)

Typical for Cast Copper High Copper Alloy

Thermal conductivity

23.0 °C

85 - 315 W/(m·K)

Show Material materials with Thermal conductivity of 85 - 315 W/(m·K)

Typical for Cast Copper High Copper Alloy

Chemical properties

PropertyValue

Aluminium

0.1 %

Show Material materials with Aluminium of 0.1 %

Beryllium

0.45 - 0.8 %

Show Material materials with Beryllium of 0.45 - 0.8 %

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

Cobalt

2.4 - 2.7 %

Show Material materials with Cobalt of 2.4 - 2.7 %

Iron

0.1 %

Show Material materials with Iron of 0.1 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Other

Rest Cu

Silicon

0.15 %

Show Material materials with Silicon of 0.15 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Zinc

0.1 %