PropertyValue

Aluminium

0.01 %

Show Material materials with Aluminium of 0.01 %

Carbon

0.1 %

Show Material materials with Carbon of 0.1 %

Copper

84.5 %

Show Material materials with Copper of 84.5 %

Iron

1.2 - 1.8 %

Show Material materials with Iron of 1.2 - 1.8 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Manganese

1.2 - 1.5 %

Show Material materials with Manganese of 1.2 - 1.5 %

Nickel

9.2 - 11 %

Show Material materials with Nickel of 9.2 - 11 %

Niobium

1 %

Show Material materials with Niobium of 1 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Zinc

0.5 %

Show Material materials with Zinc of 0.5 %