PropertyValue

Aluminium

1E-3 %

Show Material materials with Aluminium of 1E-3 %

Antimony

0.01 %

Show Material materials with Antimony of 0.01 %

Arsenic

1E-3 %

Show Material materials with Arsenic of 1E-3 %

Bismuth

0.01 %

Show Material materials with Bismuth of 0.01 %

Cadmium

0.03 %

Show Material materials with Cadmium of 0.03 %

Copper

56 - 62 %

Show Material materials with Copper of 56 - 62 %

Iron

0.25 %

Show Material materials with Iron of 0.25 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

0.2 - 1 %

Show Material materials with Manganese of 0.2 - 1 %

Nickel

0.2 - 1.5 %

Show Material materials with Nickel of 0.2 - 1.5 %

Other

Rest Zn, total 0.2. excluded Fe

Silicon

0.1 - 0.5 %

Show Material materials with Silicon of 0.1 - 0.5 %

Tin

0.5 - 1.5 %

Show Material materials with Tin of 0.5 - 1.5 %