EN 1981 Grade CM200E

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Antimony

0.2 %

Show Material materials with Antimony of 0.2 %

Arsenic

28.5 - 31.5 %

Show Material materials with Arsenic of 28.5 - 31.5 %

Bismuth

0.05 %

Show Material materials with Bismuth of 0.05 %

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

Iron

0.2 %

Show Material materials with Iron of 0.2 %

Lead

0.1 %

Show Material materials with Lead of 0.1 %

Manganese

0.2 %

Show Material materials with Manganese of 0.2 %

Other

Rest Cu, each 0.1, total 0.5

Phosphorus

0.05 %

Show Material materials with Phosphorus of 0.05 %

Selenium

0.03 %

Show Material materials with Selenium of 0.03 %

Silicon

0.1 %

Show Material materials with Silicon of 0.1 %

Tellurium

0.03 %

Show Material materials with Tellurium of 0.03 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %

Zinc

0.3 %

Show Material materials with Zinc of 0.3 %