Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
This material data has been provided by AluKey.
All categories
Let us help you find the best supplier!
Properties of Copper
List your company on Matmatch now and reach engineers around the world looking for such materials.
Request more informationChemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Copper | 57 % Show Material materials with Copper of 57 % |
Iron | 0.3 % Show Material materials with Iron of 0.3 % |
Lead | 3.5 % Show Material materials with Lead of 3.5 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Other | Rest Zn, total 0.2, in case of CuZn38Pb4 (CW609N) Pb < 4.2% |
Tin | 0.3 % Show Material materials with Tin of 0.3 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2022 Matmatch GmbH, All rights reserved.
Made with ❤️ in Munich!