Aluminum AA 2024, known for its use in aircraft industry, is an alloy that offers excellent strength. When in the annealed condition it is readily formed and has good machinability. Though it has a relatively low level of corrosion resistance, it can be machined to a high finish.

Related Standards

Equivalent Materials

This material data has been provided by AluKey.

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValueConditionRelated Standards

Density

2.78 g/cm³

Show Material materials with Density of 2.78 g/cm³

T8510

AA Standards, ASTM B241

Mechanical

PropertyValueConditionRelated StandardsComment

Elastic modulus

73.0 GPa

Show Material materials with Elastic modulus of 73.0 GPa

T8510

AA Standards, ASTM B241

Plane-Strain Fracture Toughnes

22.0 - 35.0 MPa·√m

Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m

Typical for Wrought 2000 Series Aluminium

Poisson's ratio

0.33 [-]

Show Material materials with Poisson's ratio of 0.33 [-]

Typical for Wrought 2000 Series Aluminium

Shear modulus

26.0 - 27.5 GPa

Show Material materials with Shear modulus of 26.0 - 27.5 GPa

Typical for Wrought 2000 Series Aluminium

Tensile strength

440.0 MPa

Show Material materials with Tensile strength of 440.0 MPa

T8510

AA Standards, ASTM B241

455.0 MPa

Show Material materials with Tensile strength of 455.0 MPa

T8510

AA Standards, ASTM B241

Thermal

PropertyTemperatureValueConditionRelated StandardsComment

Coefficient of thermal expansion

20 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

T8510

AA Standards, ASTM B241

100 °C

2.3199999999999998e-05 1/K

Show Material materials with Coefficient of thermal expansion of 2.3199999999999998e-05 1/K

T8510

AA Standards, ASTM B241

Melting point

505.0 - 635.0 °C

Show Material materials with Melting point of 505.0 - 635.0 °C

T8510

AA Standards, ASTM B241

Specific heat capacity

816.0 - 963.0 J/(kg·K)

Show Material materials with Specific heat capacity of 816.0 - 963.0 J/(kg·K)

Typical for Wrought 2000 Series Aluminium

Thermal conductivity

121.0 - 193.0 W/(m·K)

Show Material materials with Thermal conductivity of 121.0 - 193.0 W/(m·K)

T8510

AA Standards, ASTM B241

Electrical

PropertyValueConditionRelated Standards

Electrical conductivity

17000000.0 - 29000000.0 S/m

Show Material materials with Electrical conductivity of 17000000.0 - 29000000.0 S/m

T8510

AA Standards, ASTM B241

Electrical resistivity

3.45e-08 - 5.88e-08 Ω·m

Show Material materials with Electrical resistivity of 3.45e-08 - 5.88e-08 Ω·m

T8510

AA Standards, ASTM B241

Chemical properties

PropertyValueConditionRelated Standards

Chromium

0.1 %

Show Material materials with Chromium of 0.1 %

T8510

AA Standards, ASTM B241

Copper

3.8 - 4.9 %

Show Material materials with Copper of 3.8 - 4.9 %

T8510

AA Standards, ASTM B241

Iron

0.50 %

Show Material materials with Iron of 0.50 %

T8510

AA Standards, ASTM B241

Magnesium

1.2 - 1.8 %

Show Material materials with Magnesium of 1.2 - 1.8 %

T8510

AA Standards, ASTM B241

Manganese

0.3 - 0.9 %

Show Material materials with Manganese of 0.3 - 0.9 %

T8510

AA Standards, ASTM B241

Silicon

0.5 %

Show Material materials with Silicon of 0.5 %

T8510

AA Standards, ASTM B241

Titanium

0.15 %

Show Material materials with Titanium of 0.15 %

T8510

AA Standards, ASTM B241

Zinc

0.25 %

Show Material materials with Zinc of 0.25 %

T8510

AA Standards, ASTM B241

Technological properties

Property
Brazing

general: no brazing is known or developed

Corrosion properties

Stress corrosion cracking: Betriebsschäden in Gebieten mit Zugspannungen quer zur Kornstruktur, Eingeschränkte Schäden an Laborproben (T4,T3, T351, T3510, T3511), d (T6, T861, T81, T851, T8510, T8511), general: sufficient, in principle it should be protected

General machinability

General: poor (O), good to acceptable

Workability

general (condition): poor(T4, T3, T351, T3510, T3511, T6), not suitable (T361, T861, T81, T851, T8510, T8511)