Chemical properties
Property | Value |
---|---|
Aluminium | 0.35 - 0.4 % Show Material materials with Aluminium of 0.35 - 0.4 % |
Antimony | 0.15 % Show Material materials with Antimony of 0.15 % |
Arsenic | 0.025 - 0.05 % Show Material materials with Arsenic of 0.025 - 0.05 % |
Copper | 59 - 61.5 % Show Material materials with Copper of 59 - 61.5 % |
Iron | 0.25 % Show Material materials with Iron of 0.25 % |
Lead | 0.5 % Show Material materials with Lead of 0.5 % |
Manganese | 0.3 % Show Material materials with Manganese of 0.3 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Other | Rest Zn |
Phosphorus | 0.05 % Show Material materials with Phosphorus of 0.05 % |
Silicon | 0.05 % Show Material materials with Silicon of 0.05 % |