General
Property | Temperature | Value |
---|---|---|
Density | 23.0 °C | 7.4 g/cm³ Show Material materials with Density of 7.4 g/cm³ |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 110 - 130 GPa Show Material materials with Elastic modulus of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Elongation | 23.0 °C | 20 % Show Material materials with Elongation of 20 % | |
Hardness, Vickers | 23.0 °C | 125 [-] Show Material materials with Hardness, Vickers of 125 [-] | |
Poisson's ratio | 23.0 °C | 0.33 [-] Show Material materials with Poisson's ratio of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Tensile strength | 23.0 °C | 490 MPa Show Material materials with Tensile strength of 490 MPa | |
Yield strength Rp0.2 | 23.0 °C | 180 MPa Show Material materials with Yield strength Rp0.2 of 180 MPa |
Thermal
Property | Temperature | Value | Comment |
---|---|---|---|
Coefficient of thermal expansion | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Coefficient of thermal expansion of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Specific heat capacity | 23.0 °C | 380 J/(kg·K) Show Material materials with Specific heat capacity of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Aluminium | 8 - 9.5 % Show Material materials with Aluminium of 8 - 9.5 % |
Iron | 1 - 3 % Show Material materials with Iron of 1 - 3 % |
Lead | 0.05 % Show Material materials with Lead of 0.05 % |
Manganese | 2.5 % Show Material materials with Manganese of 2.5 % |
Nickel | 2 - 4 % Show Material materials with Nickel of 2 - 4 % |
Other | Rest Cu, total 0.3 |
Silicon | 0.1 % Show Material materials with Silicon of 0.1 % |
Tin | 0.1 % Show Material materials with Tin of 0.1 % |
Zinc | 0.2 % Show Material materials with Zinc of 0.2 % |