Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.9 g/cm³

Show Material materials with Density of 8.9 g/cm³

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Hardness, Vickers

20.0 °C

70 - 100 [-]

Show Material materials with Hardness, Vickers of 70 - 100 [-]

Tensile strength

20.0 °C

290 MPa

Show Material materials with Tensile strength of 290 MPa

Yield strength Rp0.2

20.0 °C

100 MPa

Show Material materials with Yield strength Rp0.2 of 100 MPa

Chemical properties

PropertyValue

Carbon

0.05 %

Show Material materials with Carbon of 0.05 %

Cobalt

0.1 %

Show Material materials with Cobalt of 0.1 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

24 - 26 %

Show Material materials with Nickel of 24 - 26 %

Other

Rest Cu, total 0.1

Sulfur

0.05 %

Show Material materials with Sulfur of 0.05 %

Tin

0.03 %

Show Material materials with Tin of 0.03 %

Zinc

0.5 %

Show Material materials with Zinc of 0.5 %