OUR COOKIE DISCLAIMER
Matmatch uses cookies and similar technologies to improve your experience and measure your interactions with our website. We also use them to provide you more relevant information and improve our platform and search tools. If that’s okay, click “Accept all.” To change your preferences, click “Open cookie settings.” You will find more information about cookies on our privacy policy page.
Open cookie settings
2319-F welding material
This material data has been provided by Alu Key.
All categories
We can help
you to find a supplier
We will evaluate your request for 2319-F welding material and get back to you soon.
Aircraft Aluminium Grades
Anodizing
Cast vs. Wrought Aluminium: Standards, Properties and Applications
Electrical Properties of Materials
Materials Used in Food Packaging
Precipitation Hardening (Age Hardening)
What is Bulk Modulus?
What is Creep Strength (Creep Limit)?
What is Electrical Conductivity?
What is the Coefficient of Friction?
What is the Coefficient of Thermal Expansion?
Young's Modulus: Definition, Measurement, and Typical Values
Do you supply similar materials?
List your company on Matmatch now and reach engineers around the world looking for such materials.
General
Property | Value | Temperature |
---|---|---|
Density | 2.84 g/cm³ Show Material materials with Density of 2.84 g/cm³ at 20.0 °C | 20.0 °C |
Thermal
Property | Value |
---|---|
Melting point | 543 - 643 °C Show Material materials with Melting point of 543 - 643 °C |
Chemical properties
Property | ||
---|---|---|
Copper | 6.8 % | |
Iron | 0.3 % | |
Magnesium | 0.02 % | |
Manganese | 0.4 % | |
Silicon | 0.2 % | |
Titanium | 0.2 % | |
Vanadium | 0.15 % | |
Zinc | 0.1 % | |
Zirconium | 0.25 % |
MATMATCH
We connect engineers, product designers and procurement teams with the best materials and suppliers for their job.
COMPANY
CONTACT US
+49 89 262075200
Leopoldstraße 250 A, 80807 Munich
© 2021 Matmatch GmbH, All rights reserved.
Made with ♥ in Munich!