Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.7 g/cm³

Show Material materials with Density of 8.7 g/cm³

Dimension

PropertyValue

Dimensions

Dicke

Mechanical

PropertyTemperatureValue

Elongation A50

20.0 °C

15 %

Show Material materials with Elongation A50 of 15 %

Hardness, Vickers

20.0 °C

110 - 140 [-]

Show Material materials with Hardness, Vickers of 110 - 140 [-]

Tensile strength

20.0 °C

380 - 470 MPa

Show Material materials with Tensile strength of 380 - 470 MPa

Yield strength Rp0.2

20.0 °C

260 MPa

Show Material materials with Yield strength Rp0.2 of 260 MPa

Chemical properties

PropertyValue

Copper

60 - 63 %

Show Material materials with Copper of 60 - 63 %

Iron

0.3 %

Show Material materials with Iron of 0.3 %

Lead

0.5 - 1.5 %

Show Material materials with Lead of 0.5 - 1.5 %

Manganese

0.5 %

Show Material materials with Manganese of 0.5 %

Nickel

11 - 13 %

Show Material materials with Nickel of 11 - 13 %

Other

Rest Zn, total 0.2