CEN/TS 13388 Grade CW501L R240, H050

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.8 g/cm³

Show Material materials with Density of 8.8 g/cm³

Dimension

PropertyValue

Dimensions

Dicke,Wanddicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

40 - 45 %

Show Material materials with Elongation of 40 - 45 %

Elongation A50

20.0 °C

36 %

Show Material materials with Elongation A50 of 36 %

Hardness, Brinell

20.0 °C

45 - 75 [-]

Show Material materials with Hardness, Brinell of 45 - 75 [-]

Hardness, Vickers

20.0 °C

50 - 80 [-]

Show Material materials with Hardness, Vickers of 50 - 80 [-]

Tensile strength

20.0 °C

240 - 290 MPa

Show Material materials with Tensile strength of 240 - 290 MPa

Yield strength Rp0.2

20.0 °C

140 MPa

Show Material materials with Yield strength Rp0.2 of 140 MPa

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Copper

89 - 91 %

Show Material materials with Copper of 89 - 91 %

Iron

0.05 %

Show Material materials with Iron of 0.05 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Zn, total 0.1

Tin

0.1 %