CEN/TS 13388 Grade CW619N H080

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elongation

23.0 °C

15 - 20 %

Show Material materials with Elongation of 15 - 20 %

Hardness, Brinell

23.0 °C

80 [-]

Show Material materials with Hardness, Brinell of 80 [-]

Hardness, Vickers

23.0 °C

85 [-]

Show Material materials with Hardness, Vickers of 85 [-]

Tensile strength

23.0 °C

350 - 360 MPa

Show Material materials with Tensile strength of 350 - 360 MPa

Yield strength Rp0.2

23.0 °C

120 - 140 MPa

Show Material materials with Yield strength Rp0.2 of 120 - 140 MPa

Chemical properties

PropertyValue

Aluminium

0.1 %

Show Material materials with Aluminium of 0.1 %

Copper

57 - 59 %

Show Material materials with Copper of 57 - 59 %

Iron

0.4 %

Show Material materials with Iron of 0.4 %

Lead

1.6 - 2.5 %

Show Material materials with Lead of 1.6 - 2.5 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Other

Rest Zn, total 0.2

Tin

0.2 - 0.5 %

Show Material materials with Tin of 0.2 - 0.5 %