CEN/TS 13388 Grade CW700R R380, H065

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.5 g/cm³

Show Material materials with Density of 8.5 g/cm³

Dimension

PropertyValue

Dimensions

Wanddicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

50 %

Show Material materials with Elongation of 50 %

Hardness, Brinell

20.0 °C

60 - 80 [-]

Show Material materials with Hardness, Brinell of 60 - 80 [-]

Hardness, Vickers

20.0 °C

65 - 85 [-]

Show Material materials with Hardness, Vickers of 65 - 85 [-]

Tensile strength

20.0 °C

380 MPa

Show Material materials with Tensile strength of 380 MPa

Yield strength Rp0.2

20.0 °C

115 MPa

Show Material materials with Yield strength Rp0.2 of 115 MPa

Chemical properties

PropertyValue

Copper

81 - 84 %

Show Material materials with Copper of 81 - 84 %

Iron

0.25 %

Show Material materials with Iron of 0.25 %

Lead

0.05 %

Show Material materials with Lead of 0.05 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Nickel

0.8 - 1.4 %

Show Material materials with Nickel of 0.8 - 1.4 %

Other

Rest Zn, total 0.5

Silicon

0.8 - 1.3 %

Show Material materials with Silicon of 0.8 - 1.3 %

Tin

0.1 %

Show Material materials with Tin of 0.1 %