CEN/TS 13388 Grade CW707R R340, H075

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

20.0 °C

8.5 g/cm³

Show Material materials with Density of 8.5 g/cm³

Dimension

PropertyValue

Dimensions

Wanddicke

Mechanical

PropertyTemperatureValue

Elongation

20.0 °C

45 %

Show Material materials with Elongation of 45 %

Hardness, Vickers

20.0 °C

75 - 105 [-]

Show Material materials with Hardness, Vickers of 75 - 105 [-]

Tensile strength

20.0 °C

340 MPa

Show Material materials with Tensile strength of 340 MPa

Yield strength Rp0.2

20.0 °C

130 MPa

Show Material materials with Yield strength Rp0.2 of 130 MPa

Chemical properties

PropertyValue

Aluminium

0.02 %

Show Material materials with Aluminium of 0.02 %

Arsenic

0.02 - 0.06 %

Show Material materials with Arsenic of 0.02 - 0.06 %

Copper

69 - 71 %

Show Material materials with Copper of 69 - 71 %

Iron

0.5 %

Show Material materials with Iron of 0.5 %

Lead

0.07 %

Show Material materials with Lead of 0.07 %

Manganese

0.1 %

Show Material materials with Manganese of 0.1 %

Other

Rest Zn, total 0.3

Phosphorus

0.01 %

Show Material materials with Phosphorus of 0.01 %

Tin

0.05 %

Show Material materials with Tin of 0.05 %