CEN/TS 13388 Grade CW722R R460

.XLSX
.PDF
Save

Description

Related Standards

Properties

General

Density ρ

8.3 g/cm³ at 20 °C

Dimension

Dimensions

Durchmesser

Mechanical

Elongation A

14 % at 20 °C

Elongation A100 A100

10 % at 20 °C

Hardness, Brinell HB

130 [-] at 20 °C

Hardness, Vickers HV

130 [-] at 20 °C

Tensile strength Rm

460 MPa at 20 °C

Yield strength Rp0.2 Rp0.2

250 MPa at 20 °C

Chemical properties

Element

Weight %

Comment

Other

-

Rest Zn, total 0.3

Cu

56.5 - 58.5 %

Pb

0.8 - 1.6 %

Mn

0.8 - 1.8 %

Ni

0.3 %

More

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.