GB 5233 Grade QSi3.5-3-1.5

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

100 - 125 GPa

Show Material materials with Elastic modulus of 100 - 125 GPa

Typical for Wrought Copper Brass

Shear modulus

23.0 °C

40 GPa

Show Material materials with Shear modulus of 40 GPa

Typical for Wrought Copper Brass

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.7E-5 - 2.1E-5 1/K

Show Material materials with Coefficient of thermal expansion of 1.7E-5 - 2.1E-5 1/K

Typical for Wrought Copper Brass

Melting point

875 - 1075 °C

Show Material materials with Melting point of 875 - 1075 °C

Typical for Wrought Copper Brass

Specific heat capacity

23.0 °C

371 - 418 J/(kg·K)

Show Material materials with Specific heat capacity of 371 - 418 J/(kg·K)

Typical for Wrought Copper Brass

Thermal conductivity

23.0 °C

100 - 234 W/(m·K)

Show Material materials with Thermal conductivity of 100 - 234 W/(m·K)

Typical for Wrought Copper Brass

Chemical properties

PropertyValue

Antimony

2E-3 %

Show Material materials with Antimony of 2E-3 %

Arsenic

2E-3 %

Show Material materials with Arsenic of 2E-3 %

Iron

1.2 - 1.8 %

Show Material materials with Iron of 1.2 - 1.8 %

Lead

0.03 %

Show Material materials with Lead of 0.03 %

Manganese

0.5 - 0.9 %

Show Material materials with Manganese of 0.5 - 0.9 %

Nickel

0.2 %

Show Material materials with Nickel of 0.2 %

Other

Rest Cu, total 1.1

Phosphorus

0.03 %

Show Material materials with Phosphorus of 0.03 %

Silicon

3 - 4 %

Show Material materials with Silicon of 3 - 4 %

Tin

0.25 %

Show Material materials with Tin of 0.25 %

Zinc

2.5 - 3.5 %

Show Material materials with Zinc of 2.5 - 3.5 %