GB 5233 Grade QSn4-0.3

Want to keep this datasheet? Save it now in your required format

Related Standards

This material data has been provided by AluKey.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Aluminium

2E-3 %

Show Material materials with Aluminium of 2E-3 %

Antimony

2E-3 %

Show Material materials with Antimony of 2E-3 %

Bismuth

2E-3 %

Show Material materials with Bismuth of 2E-3 %

Iron

0.02 %

Show Material materials with Iron of 0.02 %

Lead

0.02 %

Show Material materials with Lead of 0.02 %

Other

Rest Cu, total 0.1

Phosphorus

0.2 - 0.4 %

Show Material materials with Phosphorus of 0.2 - 0.4 %

Silicon

2E-3 %

Show Material materials with Silicon of 2E-3 %

Tin

3.5 - 4.5 %

Show Material materials with Tin of 3.5 - 4.5 %