Alliance Sm2Co17 SC-28

Want to keep this datasheet? Save it now in your required format

Description

Samarium Cobalt magnets are typically used in high temperature applications

This material data has been provided by Alliance LLC.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

8.4 g/cm³

Show Supplier Material materials with Density of 8.4 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

150 GPa

Show Supplier Material materials with Elastic modulus of 150 GPa

Flexural strength

23.0 °C

90 - 150 MPa

Show Supplier Material materials with Flexural strength of 90 - 150 MPa

Thermal

PropertyValue

Max service temperature

350 °C

Show Supplier Material materials with Max service temperature of 350 °C

Magnetic

PropertyTemperatureValue

Coercive force

23.0 °C

756000 A/m

Show Supplier Material materials with Coercive force of 756000 A/m

Intrinsic coercivity

23.0 °C

1.19E+6 A/m

Show Supplier Material materials with Intrinsic coercivity of 1.19E+6 A/m

Maximum energy product

23.0 °C

223 kJ/m³

Show Supplier Material materials with Maximum energy product of 223 kJ/m³

Remanence

23.0 °C

1.07 T

Show Supplier Material materials with Remanence of 1.07 T

Reversible temperature coefficient coercivity

23.0 °C

0.08 %/ °C

Show Supplier Material materials with Reversible temperature coefficient coercivity of 0.08 %/ °C

Reversible temperature coefficient remanence

23.0 °C

0.05 %/ °C

Show Supplier Material materials with Reversible temperature coefficient remanence of 0.05 %/ °C

Technological properties

Property
Application areas

Aerospace, Medical

Other

Strongest SmCo material