Description

High purity Al-Mg alloy designed to chemically brighten, accept dyes, and to anodize to an excellent uniform brightness and reflectivity.

Related Standards

Equivalent Materials

This material data has been provided by Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.68 g/cm³

Show Supplier Material materials with Density of 2.68 g/cm³

Mechanical

PropertyTemperatureValue

Elastic modulus

23.0 °C

68.6 GPa

Show Supplier Material materials with Elastic modulus of 68.6 GPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

20-100°C

Thermal conductivity

23.0 °C

146 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 146 W/(m·K)

Electrical

PropertyTemperatureValue

Electrical resistivity

23.0 °C

4.9E-8 Ω·m

Show Supplier Material materials with Electrical resistivity of 4.9E-8 Ω·m

Chemical properties

PropertyValue

Copper

0.1 %

Show Supplier Material materials with Copper of 0.1 %

Iron

0.1 %

Show Supplier Material materials with Iron of 0.1 %

Magnesium

2.2 - 2.8 %

Show Supplier Material materials with Magnesium of 2.2 - 2.8 %

Manganese

0.1 %

Show Supplier Material materials with Manganese of 0.1 %

Other

0.03 - 0.1 %

Show Supplier Material materials with Other of 0.03 - 0.1 %

Silicon

0.08 %

Show Supplier Material materials with Silicon of 0.08 %

Vanadium

0.05 %

Show Supplier Material materials with Vanadium of 0.05 %

Zinc

0.05 %

Show Supplier Material materials with Zinc of 0.05 %

Technological properties

Property
Anodizing

Very Good

Application areas

Electronic devices: Housing of devices

Corrosion properties

Excellent

Welding

Good

Workability

Very Good