8021B O Non-Heat Treatable Al Wrought Alloy

Want to keep this datasheet? Save it now in your required format

Description

Excellent formability.

Related Standards

Equivalent Materials

This material data has been provided by Aludium.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValue

Density

23.0 °C

2.72 g/cm³

Show Supplier Material materials with Density of 2.72 g/cm³

Dimension

PropertyValue

Thickness

0.09 - 0.14 mm

Show Supplier Material materials with Thickness of 0.09 - 0.14 mm

Mechanical

PropertyTemperatureValue

Elongation A50

23.0 °C

14 %

Show Supplier Material materials with Elongation A50 of 14 %

Tensile strength

23.0 °C

75 - 110 MPa

Show Supplier Material materials with Tensile strength of 75 - 110 MPa

Thermal

PropertyTemperatureValue

Coefficient of thermal expansion

100.0 °C

2.4E-5 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 2.4E-5 1/K

Chemical properties

PropertyValue

Chromium

0.03 %

Show Supplier Material materials with Chromium of 0.03 %

Copper

0.05 %

Show Supplier Material materials with Copper of 0.05 %

Iron

1.1 - 1.7 %

Show Supplier Material materials with Iron of 1.1 - 1.7 %

Magnesium

0.01 %

Show Supplier Material materials with Magnesium of 0.01 %

Manganese

0.03 %

Show Supplier Material materials with Manganese of 0.03 %

Silicon

0.4 %

Show Supplier Material materials with Silicon of 0.4 %

Titanium

0.05 %

Show Supplier Material materials with Titanium of 0.05 %

Zinc

0.05 %

Show Supplier Material materials with Zinc of 0.05 %

Technological properties

Property
Application areas

Foil stock: Foil app

Workability

Excellent