Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® 2950-05 resin is a pelletized, semi-crystalline VF2 based copolymer. It has been designed for wire and cable applications requiring high flexibility and improved resistance to impact.The low molecular weight allows extrusion conditions that reduce jacket shrink back over fiber optic constructions.

Additional characteristics:

  • Excellent thermal stability
  • Excellent abrasion resistance
  • Excellent chemical resistance
  • Impervious to UV degradation
  • High Limiting Oxygen Index
  • Extremely low smoke emission characteristics

    Meets UL910 requirements

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Abrasion resistance, weight loss

    21 - 25 mg

    Show Supplier Material materials with Abrasion resistance, weight loss of 21 - 25 mg

    ASTM-G195-13A, CS 17 1000g:pad, 1000 cycles

    Coefficient of friction, kinetic

    0.54 [-]

    Show Supplier Material materials with Coefficient of friction, kinetic of 0.54 [-]

    ASTM D1894, vs Steel

    Coefficient of friction, static

    0.55 [-]

    Show Supplier Material materials with Coefficient of friction, static of 0.55 [-]

    ASTM D1894, vs Steel

    Density

    23.0 °C

    1.78 - 1.8 g/cm³

    Show Supplier Material materials with Density of 1.78 - 1.8 g/cm³

    ASTM D792

    Limiting oxygen index

    23.0 °C

    95 %

    Show Supplier Material materials with Limiting oxygen index of 95 %

    ASTM D2863

    Water absorption

    23.0 °C

    0.03 - 0.05 %

    Show Supplier Material materials with Water absorption of 0.03 - 0.05 %

    ASTM D570

    Mechanical

    PropertyTemperatureValueComment

    Compressive strength

    23.0 °C

    24.1 - 31 MPa

    Show Supplier Material materials with Compressive strength of 24.1 - 31 MPa

    ASTM D695

    Elastic modulus

    23.0 °C

    0.28 - 0.45 GPa

    Show Supplier Material materials with Elastic modulus of 0.28 - 0.45 GPa

    ASTM D638

    Elongation

    23.0 °C

    200 - 400 %

    Show Supplier Material materials with Elongation of 200 - 400 %

    ASTM D638

    Elongation at yield

    23.0 °C

    15 - 25 %

    Show Supplier Material materials with Elongation at yield of 15 - 25 %

    ASTM D638

    Flexural modulus

    23.0 °C

    0.28 - 0.41 GPa

    Show Supplier Material materials with Flexural modulus of 0.28 - 0.41 GPa

    ASTM D790

    Hardness, Shore D

    23.0 °C

    57 - 62 [-]

    Show Supplier Material materials with Hardness, Shore D of 57 - 62 [-]

    ASTM D2240

    Tensile strength

    23.0 °C

    20 - 27.6 MPa

    Show Supplier Material materials with Tensile strength of 20 - 27.6 MPa

    ASTM D638

    Yield strength

    23.0 °C

    13.8 - 21.4 MPa

    Show Supplier Material materials with Yield strength of 13.8 - 21.4 MPa

    ASTM D638

    Impact strength, Charpy notched, ASTM

    No Break @ 23°C, ASTM D256

    Impact strength, Charpy unnotched, ASTM

    No Break @ 23°C, ASTM D256

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.62E-4 - 2.16E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.62E-4 - 2.16E-4 1/K

    ASTM D696

    Glass transition temperature

    -42.2 - -40 °C

    Show Supplier Material materials with Glass transition temperature of -42.2 - -40 °C

    ASTM D7028

    Heat deflection temperature, 0.45 MPa

    48.9 - 65.6 °C

    Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 48.9 - 65.6 °C

    ASTM D648, 248 °F/hr

    Heat deflection temperature, 1.80 MPa

    35 - 51.7 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 35 - 51.7 °C

    ASTM D648, 248 °F/hr

    Melting point

    130 - 138 °C

    Show Supplier Material materials with Melting point of 130 - 138 °C

    ASTM D3418

    Specific heat capacity

    23.0 °C

    745 - 958 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

    DSC

    Thermal conductivity

    23.0 °C

    0.14 - 0.18 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.14 - 0.18 W/(m·K)

    ASTM D433

    Thermal decomposition in air

    375 °C

    Show Supplier Material materials with Thermal decomposition in air of 375 °C

    TGA, 1% wt. loss

    Thermal decomposition in nitrogen

    410 °C

    Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

    TGA, 1% wt. loss

    Flammability

    At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 0.8 mm IEC 60695-11-10: V-0 and yellow card available

    Electrical

    PropertyTemperatureValueComment

    Dielectric constant, 1KHz

    23.0 °C

    3.8 - 12.1 [-]

    Show Supplier Material materials with Dielectric constant, 1KHz of 3.8 - 12.1 [-]

    ASTM D150

    Dielectric strength

    23.0 °C

    43.3 - 51.2 kV/mm

    Show Supplier Material materials with Dielectric strength of 43.3 - 51.2 kV/mm

    ASTM D149

    Dissipation factor, 100kHz

    23.0 °C

    0.02 - 0.24 [-]

    Show Supplier Material materials with Dissipation factor, 100kHz of 0.02 - 0.24 [-]

    ASTM D150

    Volume resistivity

    23.0 °C

    2.00E+14 Ω·cm

    Show Supplier Material materials with Volume resistivity of 2.00E+14 Ω·cm

    ASTM D257, 65% RH

    Rheological Properties

    PropertyTemperatureValueComment

    Melt mass-flow rate

    8 - 25 g/10min

    Show Supplier Material materials with Melt mass-flow rate of 8 - 25 g/10min

    ASTM D1238, 230°C/3.8kg

    Melt viscosity

    23.0 °C

    6 - 1200 Pa·s

    Show Supplier Material materials with Melt viscosity of 6 - 1200 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Automotive Cables,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables