Kynar Flex® 3030-10 America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

This material data has been provided by Arkema High Performance Polymers.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Abrasion resistance, weight loss

28 - 33 mg

Show Supplier Material materials with Abrasion resistance, weight loss of 28 - 33 mg

ASTM-G195-13A, CS 17 1000g:pad, 1000 cycles

Density

23.0 °C

1.78 - 1.82 g/cm³

Show Supplier Material materials with Density of 1.78 - 1.82 g/cm³

ASTM D792

Limiting oxygen index

23.0 °C

42 %

Show Supplier Material materials with Limiting oxygen index of 42 %

ASTM D2863

Water absorption

23.0 °C

0.5 %

Show Supplier Material materials with Water absorption of 0.5 %

max., ASTM D570

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

0.21 - 0.35 GPa

Show Supplier Material materials with Elastic modulus of 0.21 - 0.35 GPa

ASTM D638

Elongation

23.0 °C

500 %

Show Supplier Material materials with Elongation of 500 %

min., ASTM D638

Elongation at yield

23.0 °C

25 - 40 %

Show Supplier Material materials with Elongation at yield of 25 - 40 %

ASTM D638

Flexural modulus

23.0 °C

0.24 - 0.38 GPa

Show Supplier Material materials with Flexural modulus of 0.24 - 0.38 GPa

ASTM D790

Hardness, Shore D

23.0 °C

45 - 55 [-]

Show Supplier Material materials with Hardness, Shore D of 45 - 55 [-]

ASTM D2240

Tensile strength

23.0 °C

19.3 - 24.8 MPa

Show Supplier Material materials with Tensile strength of 19.3 - 24.8 MPa

ASTM D638

Yield strength

23.0 °C

12.4 - 16.5 MPa

Show Supplier Material materials with Yield strength of 12.4 - 16.5 MPa

ASTM D638

Impact strength, Charpy notched, ASTM

No Break @ 23°C, ASTM D256

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

1.53E-4 - 1.94E-4 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 1.53E-4 - 1.94E-4 1/K

ASTM D696

Glass transition temperature

-40 °C

Show Supplier Material materials with Glass transition temperature of -40 °C

ASTM D7028

Melting point

160 - 168 °C

Show Supplier Material materials with Melting point of 160 - 168 °C

ASTM D3418

Flammability

At thickness 0.8 mm IEC 60695-11-10: V-0

Electrical

PropertyTemperatureValueComment

Dielectric strength

23.0 °C

39.4 - 47.2 kV/mm

Show Supplier Material materials with Dielectric strength of 39.4 - 47.2 kV/mm

ASTM D149

Surface resistivity

23.0 °C

7.60E+11 - 7.80E+11 Ω/sq

Show Supplier Material materials with Surface resistivity of 7.60E+11 - 7.80E+11 Ω/sq

ASTM D257

Rheological Properties

PropertyTemperatureValueComment

Melt mass-flow rate

8 - 25 g/10min

Show Supplier Material materials with Melt mass-flow rate of 8 - 25 g/10min

ASTM D1238, 230°C/3.8kg

Melt viscosity

23.0 °C

700 - 1300 Pa·s

Show Supplier Material materials with Melt viscosity of 700 - 1300 Pa·s

ASTM D3835

Technological properties

Property
Application areas

Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,PVDF Cable Jacketing,Wire and Cables