Kynar Flex® 3030-15 America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® 3030-15 resin is a copolymer of vinylidene fluoride and hexafluoropropylene specifically designed for flexible plenum cables and tubing.

Its main characteristics are:

  • Very high flexibility
  • High melting point
  • Excellent low temperature impact resistance
  • Plenum rated

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Abrasion resistance, weight loss

    28 - 33 mg

    Show Supplier Material materials with Abrasion resistance, weight loss of 28 - 33 mg

    ASTM-G195-13A, CS 17 1000g:pad, 1000 cycles

    Density

    23.0 °C

    1.78 - 1.82 g/cm³

    Show Supplier Material materials with Density of 1.78 - 1.82 g/cm³

    ASTM D792

    Limiting oxygen index

    23.0 °C

    75 %

    Show Supplier Material materials with Limiting oxygen index of 75 %

    ASTM D2863

    Water absorption

    23.0 °C

    0.5 %

    Show Supplier Material materials with Water absorption of 0.5 %

    max., ASTM D570

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    0.21 - 0.35 GPa

    Show Supplier Material materials with Elastic modulus of 0.21 - 0.35 GPa

    ASTM D638

    Elongation

    23.0 °C

    500 %

    Show Supplier Material materials with Elongation of 500 %

    min., ASTM D638

    Elongation at yield

    23.0 °C

    25 - 40 %

    Show Supplier Material materials with Elongation at yield of 25 - 40 %

    ASTM D638

    Flexural modulus

    23.0 °C

    0.24 - 0.38 GPa

    Show Supplier Material materials with Flexural modulus of 0.24 - 0.38 GPa

    ASTM D790

    Hardness, Shore D

    23.0 °C

    45 - 55 [-]

    Show Supplier Material materials with Hardness, Shore D of 45 - 55 [-]

    ASTM D2240

    Tensile strength

    23.0 °C

    19.3 - 24.8 MPa

    Show Supplier Material materials with Tensile strength of 19.3 - 24.8 MPa

    ASTM D638

    Yield strength

    23.0 °C

    12.4 - 16.5 MPa

    Show Supplier Material materials with Yield strength of 12.4 - 16.5 MPa

    ASTM D638

    Impact strength, Charpy notched, ASTM

    No Break @ 23°C, ASTM D256

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.53E-4 - 1.94E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.53E-4 - 1.94E-4 1/K

    ASTM D696

    Glass transition temperature

    -40 °C

    Show Supplier Material materials with Glass transition temperature of -40 °C

    ASTM D7028

    Melting point

    160 - 168 °C

    Show Supplier Material materials with Melting point of 160 - 168 °C

    ASTM D3418

    Flammability

    At thickness 0.8 mm IEC 60695-11-10: V-0

    Electrical

    PropertyTemperatureValueComment

    Dielectric strength

    23.0 °C

    39.4 - 47.2 kV/mm

    Show Supplier Material materials with Dielectric strength of 39.4 - 47.2 kV/mm

    ASTM D149

    Surface resistivity

    23.0 °C

    7.60E+11 - 7.90E+11 Ω/sq

    Show Supplier Material materials with Surface resistivity of 7.60E+11 - 7.90E+11 Ω/sq

    ASTM D257

    Rheological Properties

    PropertyTemperatureValueComment

    Melt mass-flow rate

    8 - 25 g/10min

    Show Supplier Material materials with Melt mass-flow rate of 8 - 25 g/10min

    ASTM D1238, 230°C/3.8kg

    Melt viscosity

    23.0 °C

    700 - 1300 Pa·s

    Show Supplier Material materials with Melt viscosity of 700 - 1300 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Auto - Water Cooling Circuit,Automotive Cables,Foamed PVDF Cable Jacketing,Performance Wire,Plenum Cable,Plenum Conduit,PVDF Cable Jacketing,Wire and Cables