Kynar Flex® 3120-10 America

Alternative and trade names
PVDF
Want to keep this datasheet? Save it now in your required format

Description

Kynar Flex® resins are fluorinated thermoplastic copolymers.

Kynar Flex® 3120-10 resin is a pelletized, flexible, semi-crystalline copolymer.

Kynar Flex® 3120-10 resin is a fluid grade that can be extruded or injection molded to make final products with a 150°C rating.

Additional characteristics:

  • Excellent thermal stability
  • Excellent abrasion resistance
  • UL RTI temperature rating of 150°C
  • Impervious to UV degradation

  • This material data has been provided by Arkema High Performance Polymers.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Abrasion resistance, weight loss

    16 - 19 mg

    Show Supplier Material materials with Abrasion resistance, weight loss of 16 - 19 mg

    ASTM-G195-13A, CS 17 1000g:pad, 1000 cycles

    Coefficient of friction, kinetic

    0.3 [-]

    Show Supplier Material materials with Coefficient of friction, kinetic of 0.3 [-]

    ASTM D1894, vs Steel

    Coefficient of friction, static

    0.31 [-]

    Show Supplier Material materials with Coefficient of friction, static of 0.31 [-]

    ASTM D1894, vs Steel

    Density

    23.0 °C

    1.38 - 1.77 g/cm³

    Show Supplier Material materials with Density of 1.38 - 1.77 g/cm³

    ASTM D792

    Limiting oxygen index

    23.0 °C

    42 %

    Show Supplier Material materials with Limiting oxygen index of 42 %

    ASTM D2863

    Water absorption

    23.0 °C

    0.03 - 0.05 %

    Show Supplier Material materials with Water absorption of 0.03 - 0.05 %

    ASTM D570

    Mechanical

    PropertyTemperatureValueComment

    Compressive strength

    23.0 °C

    31 - 41.4 MPa

    Show Supplier Material materials with Compressive strength of 31 - 41.4 MPa

    ASTM D695

    Elastic modulus

    23.0 °C

    1.17 - 6.89 GPa

    Show Supplier Material materials with Elastic modulus of 1.17 - 6.89 GPa

    ASTM D638

    Elongation

    23.0 °C

    300 - 550 %

    Show Supplier Material materials with Elongation of 300 - 550 %

    ASTM D638

    Elongation at yield

    23.0 °C

    10 - 20 %

    Show Supplier Material materials with Elongation at yield of 10 - 20 %

    ASTM D638

    Flexural modulus

    23.0 °C

    0.62 - 0.83 GPa

    Show Supplier Material materials with Flexural modulus of 0.62 - 0.83 GPa

    ASTM D790

    Hardness, Shore D

    23.0 °C

    65 - 70 [-]

    Show Supplier Material materials with Hardness, Shore D of 65 - 70 [-]

    ASTM D2240

    Tensile strength

    23.0 °C

    34.5 - 48.3 MPa

    Show Supplier Material materials with Tensile strength of 34.5 - 48.3 MPa

    ASTM D638

    Yield strength

    23.0 °C

    24.1 - 34.5 MPa

    Show Supplier Material materials with Yield strength of 24.1 - 34.5 MPa

    ASTM D638

    Impact strength, Charpy notched, ASTM

    No Break @ 23°C, ASTM D256

    Impact strength, Charpy unnotched, ASTM

    No Break @ 23°C, ASTM D256

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    23.0 °C

    1.26E-4 - 1.85E-4 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 1.26E-4 - 1.85E-4 1/K

    ASTM D696

    Glass transition temperature

    -41.1 - -39.4 °C

    Show Supplier Material materials with Glass transition temperature of -41.1 - -39.4 °C

    ASTM D7028

    Heat deflection temperature, 0.45 MPa

    54.4 - 76.7 °C

    Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 54.4 - 76.7 °C

    ASTM D648, 248 °F/hr

    Heat deflection temperature, 1.80 MPa

    43.3 - 54.4 °C

    Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 43.3 - 54.4 °C

    ASTM D648, 248 °F/hr

    Melting point

    161 - 168 °C

    Show Supplier Material materials with Melting point of 161 - 168 °C

    ASTM D3418

    Relative temperature index, electrical

    150 °C

    Show Supplier Material materials with Relative temperature index, electrical of 150 °C

    UL 746B

    Relative temperature index, mechanical strength

    150 °C

    Show Supplier Material materials with Relative temperature index, mechanical strength of 150 °C

    UL 746B

    Specific heat capacity

    23.0 °C

    745 - 958 J/(kg·K)

    Show Supplier Material materials with Specific heat capacity of 745 - 958 J/(kg·K)

    DSC

    Thermal conductivity

    23.0 °C

    0.14 - 0.18 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 0.14 - 0.18 W/(m·K)

    ASTM D433

    Thermal decomposition in air

    375 °C

    Show Supplier Material materials with Thermal decomposition in air of 375 °C

    TGA, 1% wt. loss

    Thermal decomposition in nitrogen

    410 °C

    Show Supplier Material materials with Thermal decomposition in nitrogen of 410 °C

    TGA, 1% wt. loss

    Flammability

    At thickness 1.5 mm IEC 60695-11-10: V-0, At thickness 1 IEC 60695-11-10: V-0 and yellow card available, 5V at thickness 1 mm IEC 60695-11-20: 5VA

    Electrical

    PropertyTemperatureValueComment

    Dielectric constant, 1KHz

    23.0 °C

    3.2 - 10.2 [-]

    Show Supplier Material materials with Dielectric constant, 1KHz of 3.2 - 10.2 [-]

    ASTM D150

    Dielectric strength

    23.0 °C

    51.2 - 59.1 kV/mm

    Show Supplier Material materials with Dielectric strength of 51.2 - 59.1 kV/mm

    ASTM D149

    Dissipation factor, 100kHz

    23.0 °C

    0.02 - 0.19 [-]

    Show Supplier Material materials with Dissipation factor, 100kHz of 0.02 - 0.19 [-]

    ASTM D150

    Optical

    PropertyValueComment

    Refractive index

    1.41 [-]

    Show Supplier Material materials with Refractive index of 1.41 [-]

    ASTM D542, sodium D line

    Rheological Properties

    PropertyTemperatureValueComment

    Melt mass-flow rate

    4 - 12 g/10min

    Show Supplier Material materials with Melt mass-flow rate of 4 - 12 g/10min

    ASTM D1238, 230°C/3.8kg

    Melt viscosity

    23.0 °C

    500 - 1300 Pa·s

    Show Supplier Material materials with Melt viscosity of 500 - 1300 Pa·s

    ASTM D3835

    Technological properties

    Property
    Application areas

    Cable Ties,Chemical Process Industry - Injection Molding